Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.40 MPa @Temperature 23.0 °C |
5425 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H07B-00 Polypropylene Homopolymer This is a polypropylene homopolymer for cast film applications that require antiblock additives. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 17.. |