Tensile Strength, Yield 525 MPa

@Strain 0.200 %,
Temperature 650 °C
76100 psi

@Strain 0.200 %,
Temperature 1200 °F
Haynes 214® alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 525 MPa

@Strain 0.200 %
76100 psi

@Strain 0.200 %
Haynes 230® alloy, 30% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Yield 525 MPa

@Strain 0.200 %
76100 psi

@Strain 0.200 %
Haynes 230® alloy, 40% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Yield 525 MPa
76100 psi
Haynes Hastelloy® W alloy, shielded metal arc welds, as-welded
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 525 MPa

@Strain 0.200 %,
Temperature 650 °C
76100 psi

@Strain 0.200 %,
Temperature 1200 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
Tensile Strength, Yield 525 MPa

@Strain 0.200 %
76100 psi

@Strain 0.200 %
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 20% Cold Work
Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 9.0. Other property values are typical of t..
Tensile Strength, Yield 525 MPa

@Strain 0.200 %,
Temperature 650 °C
76100 psi

@Strain 0.200 %,
Temperature 1200 °F
Haynes 242® alloy, hot rolled plate, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal..