Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 352 MPa @Strain 0.200 % |
51100 psi @Strain 0.200 % |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 352 MPa @Strain 0.200 %, Thickness 9.50 mm |
51100 psi @Strain 0.200 %, Thickness 0.374 in |
plate |
AK Steel 409Ni Ferritic Stainless steel AK Steel 409Ni is a nominal 11% chromium stainless steel micro-alloyed with titanium, manganese and nickel that provides excellent weldability, toughness and fabricating characteristics. AK Steel 4.. |
|||
Tensile Strength, Yield | 352 MPa @Strain 0.200 %, Temperature 260 °C |
51100 psi @Strain 0.200 %, Temperature 500 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |