Material Notes:
AK Steel 409Ni is a nominal 11% chromium stainless steel micro-alloyed with titanium, manganese and nickel that provides excellent weldability, toughness and fabricating characteristics. AK Steel 409Ni is an ideal material for applications requiring weldability and toughness superior to standard Type 409, at relatively low cost.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 83

@Thickness 9.50 mm
83

@Thickness 0.374 in
plate
Tensile Strength, Ultimate 469 MPa

@Thickness 9.50 mm
68000 psi

@Thickness 0.374 in
plate
Tensile Strength, Yield 352 MPa

@Strain 0.200 %,
Thickness 9.50 mm
51100 psi

@Strain 0.200 %,
Thickness 0.374 in
plate
Elongation at Break 28 %
28 %
in 2 inches, 9.5 mm plate
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 11 %
11 %
Iron, Fe 86.841 %
86.841 %
As Remainder
Manganese, Mn 0.70 %
0.70 %
Nickel, Ni 0.85 %
0.85 %
Nitrogen, N 0.015 %
0.015 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.35 %
0.35 %
Sulfur, S 0.0040 %
0.0040 %
Titanium, Ti 0.20 %
0.20 %