Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 348 MPa @Strain 0.200 % |
50500 psi @Strain 0.200 % |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 348 MPa @Strain 0.200 % |
50500 psi @Strain 0.200 % |
|
Special Metals INCONEL® 690 Nickel Superalloy, Cold Rolled Strip, 0.150 inch (3.81 mm) Thick Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and.. |
|||
Tensile Strength, Yield | 348 MPa @Strain 0.200 %, Thickness 3.20 mm |
50500 psi @Strain 0.200 %, Thickness 0.126 in |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |