Polymer Property : Tensile Strength, Yield = 5.78 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.78 MPa
839 psi
at 200%, post cured- 2 hours at 177°C; ASTM D412
Multibase C6-570 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 5.78 MPa
839 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5723 Fluorocarbon-Elastomer
Formulated Viton®. General service.Information provided by Seals Eastern, Inc.