Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.30 MPa | 769 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 5514 Polyacrylate Rubber General purpose Natural RubberInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 5.30 MPa @Strain 100 % |
769 psi @Strain 100 % |
|
Daikin DAI-EL G-701 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent compression set.Information provided by.. |
|||
Tensile Strength, Yield | 5.30 MPa | 769 psi | 50 microns film; ASTM D882 |
Arkema Group Orevac® 9314 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Blown film coextrusionInformation provided by Arkema Group |