Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.10 MPa

@Temperature -55.0 °C
740 psi

@Temperature -67.0 °F
Flatwise Tensile; 2.52" Cell; Aluminum Honeycomb Sandwich Performance; ASTM C 297
Hexcel® Redux® HP655 Toughened BMI film Adhesive
Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655..
Tensile Strength, Yield 5.10 MPa

@Temperature 21.1 °C
740 psi

@Temperature 70.0 °F
Flatwise Tensile; 2.52" Cell; Aluminum Honeycomb Sandwich Performance; ASTM C 297
Hexcel® Redux® HP655 Toughened BMI film Adhesive
Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655..
Tensile Strength, Yield 5.10 MPa

@Strain 100 %
740 psi

@Strain 100 %
Daikin DAI-EL G-671 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 67% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Excellent low-temperature sealing ..
Tensile Strength, Yield 5.10 MPa
740 psi
ASTM D638
Arkema Group OREVAC® 18211 Maleic Anhydride Grafted EVA Copolymer
OREVAC® 18211 is maleic anhydride grafted EVA copolymer. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. ORE..
Tensile Strength, Yield 5.10 MPa
740 psi
M100
3M Dyneon™ Fluorel™ FC-2260 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl ..