Material Notes:
OREVAC® 18211 is maleic anhydride grafted EVA copolymer. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 18211 provides outstanding adhesion to PS, PE, PA, EVOH. It is typically used in coextrusion of multilayer structures used in flexible or rigid packaging.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183
Melt Index of Compound 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 27
27
ISO 608
Tensile Strength at Break 29.3 MPa
4250 psi
Tensile Strength, Yield 5.10 MPa
740 psi
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Dart Drop Test 260 g
0.573 lb
ASTM D1709
Thermal Properties Metric English Comments
Melting Point 75.0 °C
167 °F
DSC
Vicat Softening Point 51.0 °C
124 °F
ISO 306
Optical Properties Metric English Comments