Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 33.0 MPa | 4780 psi | molded and tested in accordance with ASTM D 4101; ASTM D638 |
Dow DX5E66 Polypropylene Resin DOW DX5E66 is intended for use in cast film processes.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |