Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.6 MPa
4730 psi
78% Ret.
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 32.6 MPa
4730 psi
ASTM D638
Diamond Polymers NPP50-1111 TF20 20% Talc Filled White High Density Polyethylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.