Diamond Polymers NPP50-1111 TF20 20% Talc Filled White High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP50-1111 TF20 20% Talc Filled White High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D1505
Melt Flow 0.10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
29.8 g/10 min

@Load 21.6 kg,
Temperature 190 °C
29.8 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.6 MPa
4730 psi
ASTM D638
Elongation at Break >= 110 %
>= 110 %
ASTM D638
Flexural Strength 29.3 MPa
4250 psi
ASTM D790
Flexural Modulus 1.516 GPa
219.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 89.6 °C
193 °F
0.125";; ASTM D648
Vicat Softening Point 126 °C
259 °F
ASTM D1525