Polymer Property : Tensile Strength, Yield = 47.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.2 MPa
6850 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Dry Blend E7130 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 47.2 MPa
6850 psi
ASTM D638
Spartech CastAlloy Weatherable Sheet
Description: Weatherable SheetInformation provided by Spartech.
Tensile Strength, Yield 47.2 - 47.6 MPa
6850 - 6900 psi
ASTM D638M
DSM Somos® GP Plus 14122
Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually ..