Polymer Property : Tensile Strength, Yield = 46.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.5 MPa
6740 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 01FG Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 46.5 MPa
6740 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 13FG Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 46.5 MPa
6740 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87358 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Strength, Yield 46.5 MPa
6750 psi
ASTM D638
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 46.5 MPa
6740 psi
ASTM D368
Reliance Industries PVAXX H65
The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie..
Tensile Strength, Yield 46.5 MPa
6740 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..