Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 313 MPa @Strain 0.200 %, Temperature 816 °C |
45400 psi @Strain 0.200 %, Temperature 1500 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Tensile Strength, Yield | 313 MPa @Strain 0.200 % |
45400 psi @Strain 0.200 % |
Typical Annealed |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed) Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci.. |
|||
Tensile Strength, Yield | 313 MPa @Strain 0.200 % |
45400 psi @Strain 0.200 % |
typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Annealed Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |