Mechanical Properties Metric English Comments
Tensile Strength, Yield 308 MPa

@Temperature 24.0 °C
44700 psi

@Temperature 75.2 °F
Warp TS
Hexcel® HexPly® F185 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F185; Fiber: 450-1/2Information provided by HexCel
Tensile Strength, Yield 308 MPa

@Strain 0.200 %
44700 psi

@Strain 0.200 %
Haynes Hastelloy® N, 1.14 mm sheet, heat treated at 1149°C (2100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..