Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.23 MPa
4384 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR Di-Cup 40C Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tensile Strength, Yield 30.23 MPa
4384 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 30.23 MPa
4384 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 30.23 MPa
4384 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR Di-Cup 40C Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..