Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.96 MPa | 430 psi | at 200%, molded-without post cure; ASTM D412 |
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.96 MPa | 430 psi | ASTM D638 |
Dow AMPLIFY™ EA 101 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 101 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |
|||
Tensile Strength, Yield | 2.96 MPa | 430 psi | ASTM D638 |
Dow AMPLIFY™ EA 102 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 102 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |