Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 430 MPa
>= 62400 psi
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T6
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Tensile Strength, Yield 430 MPa
62400 psi
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 625/ Alloy 718 12.7 mm plate weldments
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 430 MPa

@Strain 0.200 %
62400 psi

@Strain 0.200 %
Haynes 556® alloy, bar, after 0 hours at 650°C (1200°F)
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Yield >= 430 MPa

@Strain 0.200 %
>= 62400 psi

@Strain 0.200 %
Schmolz + Bickenbach UGICHROM 4362 Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Copyright © lookpolymers.com All Rights Reserved