Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.207 - 29.0 MPa | 30.0 - 4210 psi | Average value: 3.62 MPa Grade Count:320 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tensile Strength, Yield | 23.0 - 29.0 MPa | 3340 - 4210 psi | Average value: 26.7 MPa Grade Count:3 |
Overview of materials for Polystyrene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Wood Filled". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tensile Strength, Yield | 27.0 - 29.0 MPa | 3920 - 4210 psi | MD/TD; ISO 527-2 |
Borealis HB205TF Polypropylene HB205TF is a low melt flow rate polypropylene homopolymer intended for extrusion, calendering and thermoforming. Its very good organoleptic properties allows this grade to be used with any master b.. |