Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.83 MPa @Strain 300 % |
410 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Synprene® RT-3770 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength, Yield | 2.83 MPa | 410 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® E38 Perfluoroelastomer Chemraz® E38 was specifically developed for high-density plasma systems and diffusion processes where seal reliability and very minimal contamination are essential. The material provides excelle.. |
|||
Tensile Strength, Yield | 2.83 MPa | 410 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-150 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.83 MPa | 410 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7345 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.83 MPa | 410 psi | 100%; ASTM D412 |
Teknor Apex APEX® 1519-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsFeatures- Good flexibility Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 2.83 MPa @Strain 300 % |
410 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 37-033 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A therm.. |