Greene Tweed CHEMRAZ® E38 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® E38 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemraz® E38 was specifically developed for high-density plasma systems and diffusion processes where seal reliability and very minimal contamination are essential. The material provides excellent chemical compatibility and withstands a variety of aggressive chemicals. Available in an infinite range of geometries and cross sections, this material offers the diversity required for a variety of dynamic or static dry processing applications. Recommended for slit valves, Chemraz E38 remains stable at service temperatures as high as 260°C (500°F) where high sealing loads are not used.Applications:Bonded gate sealsChamber sealsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.99 g/cc
1.99 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
ASTM D1414
Tensile Strength, Yield 2.83 MPa
410 psi
@50% Elongation; ASTM D1414
7.58 MPa
1100 psi
@100% Elongation; ASTM D1414
Elongation at Break 150 %
150 %
ASTM D1414
Compression Set 21 %
21 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Descriptive Properties Value Comments
Color White