Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 274 MPa @Strain 0.200 %, Temperature 538 °C |
39700 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |