Polymer Property : Tensile Strength, Yield = 393 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 393 MPa

@Strain 0.200 %
57000 psi

@Strain 0.200 %
PSM Industries PolyAlloys MIM-Fe-%3Si Grade 2 Soft Magnetic Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
Tensile Strength, Yield 393 MPa

@Diameter 12.7 mm
57000 psi

@Diameter 0.500 in
Kaiser 6033 T6, T651 Rod & Bar
Alloy 6033 is a higher strength version of alloy 6061, approaching properties typically obtainable with 2000 series alloys. The alloy was developed to also offer improved machinability over 6061. Th..
Tensile Strength, Yield 393 MPa

@Strain 0.200 %
57000 psi

@Strain 0.200 %
Haynes Multimet® alloy, 1.32 mm thick sheet, 1177°C heat treatment, rapid air cooled
Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit..
Tensile Strength, Yield 393 MPa

@Diameter 12.7 mm
57000 psi

@Diameter 0.500 in
Kaiser 4026 T651 Rod & Bar
This alloy is used when high strength with wear and/or galling resistance is required. It can eliminate hard-coat anodizing in some applications. Typical applications include air compressor pistons ..
Tensile Strength, Yield 393 MPa

@Strain 0.200 %
57000 psi

@Strain 0.200 %
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Yield 393 MPa

@Strain 0.200 %
57000 psi

@Strain 0.200 %
HP Alloys Nitronic® 50 Austenitic Stainless, Annealed
Annealed applies to tensile, impact, and hardness values and are for 3/4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of co..
Tensile Strength, Yield 393 MPa

@Strain 0.200 %
57000 psi

@Strain 0.200 %
Universal Wire Works 2319 (AMS 4191) Aluminum Alloy Filler Metal
Alloy 2319 is used on applications requiring good strength at high temperatures (600°F) and many cryogenic and aircraft parts. Primarily used where weld joints are capable of being heat treated to ..
Tensile Strength, Yield 393 - 434 MPa
57000 - 63000 psi
0.2% offset
Eagle Brass 151 ZHC® COPPER, Extra Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Tensile Strength, Yield 393 - 476 MPa
57000 - 69000 psi
0.2% offset
Eagle Brass 230 Red Brass, Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Yield 393 MPa

@Strain 0.200 %
57000 psi

@Strain 0.200 %
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 843°C
Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l..
Tensile Strength, Yield 393 MPa

@Strain 0.200 %
57000 psi

@Strain 0.200 %
PSM Industries PolyAlloys MIM-Fe-%3Si Grade 1 Soft Magnetic Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
Tensile Strength, Yield 393 MPa

@Strain 0.200 %,
Temperature 538 °C
57000 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..