PSM Industries PolyAlloys MIM-Fe-%3Si Grade 1 Soft Magnetic Steel

Category Metal , Electronic/Magnetic Alloy
Manufacturer PSM Industries
Trade Name PolyAlloys
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries PolyAlloys MIM-Fe-%3Si Grade 1 Soft Magnetic Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of complexity and near full theoretical density by utilizing Metal Injection Molding (MIM).  MIM can economically produce complex shapes beyond the capability of conventional Powdered Metallurgy.Benefits of Metal Injection Molding96-98% of Theoretical DensityExcellent Mechanical PropertiesAvoids Costly Secondary OperationsExcellent Surface FinishesCapable of Extreme 3-D GeometriesHolds Tight TolerancesExtremely Thin Wall Section CapabilitiesInformation Provided by PolyAlloys, a division of PSM Industries
Physical Properties Metric English Comments
Density 7.60 g/cc
0.275 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80
80
Macro
Tensile Strength, Ultimate 531 MPa
77000 psi
Tensile Strength, Yield 393 MPa

@Strain 0.200 %
57000 psi

@Strain 0.200 %
Elongation at Yield 24 %
24 %
in 1 in.
Electrical Properties Metric English Comments
Magnetic Permeability >= 8000
>= 8000
8500
8500
Typical
Magnetic Coercive Force, Hc 0.70 Oe
0.70 Oe
Magnetic Remanence, Br 12000 Gauss
12000 Gauss
Descriptive Properties Value Comments
B25 (kG) 14
min
14.5
Typical
B500 (kG) 19.5