Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.70 MPa | 391 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-540 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.70 MPa | 391 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7284 Butyl and Halobutyl Rubber Chlorobutyl; High damping; Non-conductiveInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.70 MPa | 391 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 5404 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |