Polymer Property : Tensile Strength, Yield = 386 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.66 MPa
386 psi
Fujipoly Industries Sarcon® 30Q Thin-Film QR
Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
Tensile Strength, Yield 2.66 MPa
386 psi
Fujipoly Industries Sarcon® 45U Thin-Film UR
Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..