Polymer Property : Tensile Strength, Yield = 380 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.62 MPa
380 psi
at 200%, no post cure- press cured for 5 minutes; ASTM D412
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Yield 2.62 MPa
380 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-UR-110-W Polyurethane, Unspecified (PUR, Unspecified)
Information provided by PolyOne
Tensile Strength, Yield 2.62 MPa
380 psi
ASTM D412
Polymax® Maxelast® P2750 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 2.62 MPa
380 psi
@100% Elongation; ASTM D1414
Greene Tweed FLUORAZ® 784 Fluoroelastomer, FEPM
Sanitary gaskets made from Fluoraz® 784 work well in Sip and CIP applications where a low durometer elastomer compound is needed. While EPDMs and FKMs can provide a seal for extended periods, ch..
Tensile Strength, Yield 2.62 MPa
380 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5242 Neoprene / Chloroprene
General purpose neopreneInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield >= 2.62 MPa
>= 380 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7265D Fluorocarbon-Elastomer
Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 2.62 MPa
380 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7282 Neoprene / Chloroprene
UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 2.62 MPa
380 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7336 Highly Saturated Nitrile Rubber
HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 2.62 MPa

@Strain 300 %
380 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 36-021 NATURAL Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Specialty Thermoplastic ElastomerApplications: FDA (Food Contact)Processing Method: Injection MoldingInformation provided by PolyOne Corporation