Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.5 - 29.4 MPa | 3560 - 4270 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Tensile Strength, Yield | 24.5 - 29.4 MPa | 3560 - 4270 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | ASTM D638 |
ExxonMobil HD 6761.17 Injection Molding Resin
(discontinued **) HD 6761 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a heavy-d.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® M4621 High Density Polyethylene ApplicationsALATHON M 4621 is a copolymer that provides outstanding stress crack resistance and low temperature impact strength. Typical applications include small two-piece engine gas tanks, waste.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | ASTM D638 |
Hyosung Topilene HJ646 PP HJ646 Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | ASTM D638 |
Hyosung Topilene HJ746 PP HJ746 Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 24.5 MPa @Thickness 3.20 mm |
3560 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Tensile Strength, Yield | 24.5 MPa @Thickness 3.20 mm |
3560 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HI5204S PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 24.5 MPa @Thickness 3.20 mm |
3560 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HI5205R PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 24.5 MPa @Thickness 3.20 mm |
3560 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HI5302R PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | 50 mm/min; ASTM D638 |
LG Chemical SEETEC PM360 HDPE Features: Characteristics: Excellent processability, Good tenacity & knot strengthAdditives: Anti-oxidants, LubricantsApplication: Tarpaulin, Woven bags (Inflation)CAS No. 25213-02-9Information prov.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | |
Microcell Composite Company CELLIFF® 7000 Polymer Pellets CELLIFF® special high polymer materials are mixed for high degrees of hardness and tenacity. For producing stiff, light weight foaming boards which are tenacious and durable. The foam surface can.. |
|||
Tensile Strength, Yield | 24.5 MPa @Thickness 3.20 mm |
3560 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | ASTM D638M |
Total PSI 4440(AS) High Impact Polystyrene 4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, .. |
|||
Tensile Strength, Yield | 24.5 MPa | 3560 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |