Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 - 29.4 MPa
3560 - 4270 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE)
POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of ..
Tensile Strength, Yield 24.5 - 29.4 MPa
3560 - 4270 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE)
POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of ..