Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.27 MPa | 3375 psi | ASTM D638 |
Washington Penn Medium Impact Copolymer 20% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |