Tensile Strength, Yield 23.27 MPa
3375 psi
ASTM D638
Washington Penn Medium Impact Copolymer 20% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..