Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.9 MPa | 3320 psi | ASTM D412 |
Polymax® Maxelast® P3896 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 22.9 MPa | 3320 psi | ASTM D638 |
ExxonMobil HD 6714.17 Injection Molding Resin
(discontinued **) HD 6714 is a narrow molecular weight hexene copolymer designed for outstanding processability to maximize injection molding productivity. This resin is ideally suited for thin wall multicavity part.. |
|||
Tensile Strength, Yield | 22.9 MPa | 3320 psi | Result |
Westlake Plastics Lennite® GUR1020 (Type I) Ultra-high Molecular Weight Polyethylene For Medical Applications Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m.. |