Polymer Property : Tensile Strength, Yield = 22.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.9 MPa
3320 psi
ASTM D412
Polymax® Maxelast® P3896 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 22.9 MPa
3320 psi
ASTM D638
ExxonMobil HD 6714.17 Injection Molding Resin  (discontinued **)
HD 6714 is a narrow molecular weight hexene copolymer designed for outstanding processability to maximize injection molding productivity. This resin is ideally suited for thin wall multicavity part..
Tensile Strength, Yield 22.9 MPa
3320 psi
Result
Westlake Plastics Lennite® GUR1020 (Type I) Ultra-high Molecular Weight Polyethylene For Medical Applications
Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m..