Polymer Property : Tensile Strength, Yield = 316 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.18 MPa
316 psi
ASTM D412
Polymax® Maxelast® C4912 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Strength, Yield >= 2.18 MPa
>= 316 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7027 Butyl and Halobutyl Rubber
General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 2.18 MPa
316 psi
at 100% elongation, maximum
Dow Corning SILASTIC® 25786-V SILICONE RUBBER RED
60 Durometer, peroxide cured, high temperature resistance Silicone Rubber CompoundInformation provided by Dow Corning
Tensile Strength, Yield >= 2.18 MPa
>= 316 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5403 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.