Dow Corning SILASTIC® 25786-V SILICONE RUBBER RED

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 25786-V SILICONE RUBBER RED.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
60 Durometer, peroxide cured, high temperature resistance Silicone Rubber CompoundInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc

@Temperature 25.0 °C
1.20 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
Tensile Strength, Ultimate 7.460 MPa
1082 psi
Tensile Strength, Yield 2.18 MPa
316 psi
at 100% elongation, maximum
Elongation at Break 294 %
294 %
Tear Strength 14.4 kN/m
82.0 pli
Descriptive Properties Value Comments
Color red