Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 31.11 MPa | 4512 psi | 150°C for 1,000 hrs; ASTM D1458 |
Fujipoly Industries Sarcon® 45GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |