Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2070 MPa | 300000 psi | ASTM D3039 |
Greene Tweed WR™ 525 PEEK, Carbon Filled WR®525 is a thermoplastic composite consisting of carbon fiber in a PEEK matrix. Because of its unique thermal expansion properties, WR525 is deal for use as impeller wear rings, bushings and ca.. |