Polymer Property : Tensile Strength, Yield = 2070 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2070 MPa
300000 psi
ASTM D3039
Greene Tweed WRâ„¢ 525 PEEK, Carbon Filled
WR®525 is a thermoplastic composite consisting of carbon fiber in a PEEK matrix. Because of its unique thermal expansion properties, WR525 is deal for use as impeller wear rings, bushings and ca..