Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 19.00 MPa | 2756 psi | 2 in/min; LAB032 |
ExxonMobil Mytex™ AS33L-07VS rubber modified polypropylene with good impact and flow properties for automotive exterior applications.Information provided by ExxonMobil Chemical |