Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 19.00 MPa | 2755 psi | At 50 mm/min; ISO 527-2 |
Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor.. |
|||
Tensile Strength, Yield | 19.00 MPa | 2755 psi | At 50 mm/min; ISO 527-2 |
Borealis Borstar® ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes Borstar ME3441 is a yellow, bimodal, cadmium free, medium density polyethylene compound classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. It includes a combinat.. |
|||
Tensile Strength, Yield | 19.00 MPa | 2755 psi | Cable At 50 mm/min; IEC 60811-1-1 |
Borealis Casico™ FR4805 Non Halogen Flame Retardant Compound for Sheathing Energy Cables Casico FR4805 is a thermoplastic, non-halogen containing natural jacketing compound. It combines high mechanical strength and toughness with flame retardancy. The composition of Casico FR4805 is b.. |
|||
Tensile Strength, Yield | 19.00 MPa | 2756 psi | 2 in/min; LAB032 |
ExxonMobil Mytex™ AS33L-07VS rubber modified polypropylene with good impact and flow properties for automotive exterior applications.Information provided by ExxonMobil Chemical |
|||
Tensile Strength, Yield | 19.00 MPa | 2755 psi | ISO 527-2 |
Borealis Borstar® ME3444 Blue Medium Density Polyethylene for Drinking Water Pipes Borstar 3444 is a blue, bimodal, medium density polyethylene classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. A combination of pigments and stabilizers is incl.. |