Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1600 - 1640 MPa | 232000 - 238000 psi | |
Plansee DENAL® 910 179 20 Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |
|||
Tensile Strength, Yield | 1600 MPa | 232000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Tensile Strength, Yield | 1600 MPa | 232000 psi | when tempered at 1000°F |
Carpenter No. 883® Hot Work Die Steel (Red-Tough) (AISI H13) No. 883 hot work die steel is a 5% chromium hot work tool steel designed particularly for applications requiring extreme toughness combined with good red-hardness. It has given an extra margin of sa.. |