Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1.59 MPa | >= 231 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5433 Nitrile Rubber General purpose Nitrile; Low water swellInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.59 MPa | 231 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 5722 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |