Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.57 MPa | 228 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® T460AH Thermoplastic Polyurethane Type: Estane® T460AH is a Shore 60A, polyester grade, plasticizer-free, with low hardness and Hydrolytic Stabilizer thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: Americas, .. |