Lubrizol Estane® T460AH Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® T460AH Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® T460AH is a Shore 60A, polyester grade, plasticizer-free, with low hardness and Hydrolytic Stabilizer thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength, Ultimate 18.6 MPa
2700 psi
ASTM D412
Tensile Strength, Yield 1.57 MPa
228 psi
at 100% elongation; ASTM D412
2.55 MPa
370 psi
at 300% elongation; ASTM D412
Elongation at Break 1000 %
1000 %
ASTM D412
Tear Strength 47.1 kN/m
269 pli
Die C; ASTM D624
Abrasion 64
64
ASTM D4649
Thermal Properties Metric English Comments
Vicat Softening Point 70.0 °C
158 °F
ASTM D1525