Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.57 MPa | 227 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit.. |