Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1531 MPa | 222100 psi | Longitudinal |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 13.5 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Tensile Strength, Yield | 1531 MPa | 222100 psi | Hardened 1900°F, Tempered 600°F |
ATI Allegheny Ludlum 440A Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 1531 MPa @Strain 0.200 % |
222100 psi @Strain 0.200 % |
typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 316°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |