Polymer Property : Tensile Strength, Yield = 1531 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1531 MPa
222100 psi
Longitudinal
Latrobe Lescalloy® AF 1410 VIM-VAR ; 13.5 in High Strength Alloy Steel
LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical,..
Tensile Strength, Yield 1531 MPa
222100 psi
Hardened 1900°F, Tempered 600°F
ATI Allegheny Ludlum 440A Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Tensile Strength, Yield 1531 MPa

@Strain 0.200 %
222100 psi

@Strain 0.200 %
typical
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 316°C Temper
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..