Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.9 MPa | 2160 psi | ASTM D412 |
Polymax® Maxelast® F7890 TPE, Fire Retardant Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome.. |
|||
Tensile Strength, Yield | 14.9 MPa | 2160 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G60A Perfluoroelastomer A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Suitable for app.. |
|||
Tensile Strength, Yield | 14.9 MPa | 2160 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G80X Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require exposure.. |
|||
Tensile Strength, Yield | 14.9 MPa | 2160 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Cellular E2000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 14.9 MPa | 2160 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Cellular E2001 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 14.9 MPa | 2160 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Cellular E2010 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Physical Properties were measured on flat cellular profiles with a 0.59 specific gravity natural compound.Information provided by PolyOne |
|||
Tensile Strength, Yield | 14.9 MPa | 2160 psi | Change in tensile strength after 504 hours at 248°F; ASTM D638 |
Teknor Apex Sinvicomp SIH 7005A Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness; High Heat Resistance Uses: Wire and Cable Applications Wire Types: V-90HT Agency Ratings: AS 3147-1992 Forms: Pellets Processing Method: Extrusio.. |
|||
Tensile Strength, Yield | 14.9 MPa | 2160 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 1721-xx14E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |