Polymer Property : Tensile Strength, Yield = 14.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.9 MPa
2160 psi
ASTM D412
Polymax® Maxelast® F7890 TPE, Fire Retardant
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome..
Tensile Strength, Yield 14.9 MPa
2160 psi
ASTM D412
Precision Polymer Engineering Perlast® G60A Perfluoroelastomer
A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Suitable for app..
Tensile Strength, Yield 14.9 MPa
2160 psi
ASTM D412
Precision Polymer Engineering Perlast® G80X Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require exposure..
Tensile Strength, Yield 14.9 MPa
2160 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Cellular E2000 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 14.9 MPa
2160 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Cellular E2001 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 14.9 MPa
2160 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Cellular E2010 Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Physical Properties were measured on flat cellular profiles with a 0.59 specific gravity natural compound.Information provided by PolyOne
Tensile Strength, Yield 14.9 MPa
2160 psi
Change in tensile strength after 504 hours at 248°F; ASTM D638
Teknor Apex Sinvicomp SIH 7005A Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Good Stiffness; High Heat Resistance Uses: Wire and Cable Applications Wire Types: V-90HT Agency Ratings: AS 3147-1992 Forms: Pellets Processing Method: Extrusio..
Tensile Strength, Yield 14.9 MPa
2160 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable 1721-xx14E Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne